dc.description.abstract | In the concrete structures exposed to environmental conditions at early ages, water movement occurs by moisture diffusion in the concrete, and self-desiccation of concrete is also occurred. Thus the internal relative humidity is changed from moisture diffusion and self-desiccation. Thus the internal relative humidity at each location in concrete includes the decrease by self-desiccation. Especially, for high-strength concrete the much unit cement content is used, so that the non-uniform relative humidity distribution is affected form self-desiccation at early ages. In this study, the internal relative humidity in concrete was measured at early ages, and the moisture diffusion component and self-desiccation component of total relative humidity were discussed. | - |
dc.language | KOR | - |
dc.publisher | 한국콘크리트학회 | - |
dc.title | 초기재령 콘크리트의 수분확산과 자체건조에 관한 연구 | - |
dc.title.alternative | Moisture Diffusion and Self-desiccation of Concrete at Early Ages | - |
dc.type | Conference | - |
dc.type.rims | CONF | - |
dc.citation.beginningpage | 303 | - |
dc.citation.endingpage | 308 | - |
dc.citation.publicationname | 1998 한국콘크리트학회 봄 학술대회 | - |
dc.identifier.conferencecountry | South Korea | - |
dc.identifier.conferencecountry | South Korea | - |
dc.contributor.localauthor | 김진근 | - |
dc.contributor.nonIdAuthor | 이칠성 | - |
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.