Electro-optical and Electrochemical Properties of Poly(1-hexyne)

Cited 3 time in webofscience Cited 0 time in scopus
  • Hit : 403
  • Download : 0
Poly(1-hexyne) was prepared by the polymerization of 1-hexyne by using transition metal catalyst. The instrumental analysis data on the polymer structure revealed that the poly(1-hexyne) have the conjugated polyene backbone structure with n-butyl substituents. Poly(1-hexyne) showed UV-visible absorption band at 276 nm and PL spectrum at 415 nm, indicating relatively blue-shifted PL maximum value. From the relationship plot of the oxidation current density (log i(p),(a)) as a function of the scan rate (log v), it was found that the oxidation current of poly(1-hexyne) versus the scan rate is approximately linear relationship in the range of 30 similar to 150 mV/sec and the exponent of scan rate, x value is found to be 0.424. It is explained by that the kinetics of the redox process are close to the diffusion-control process. The band gap energy of poly(1-hexyne) was estimated to be 2.98 eV and HOMO and LUMO level values of poly(1-hexyne) were 5.35 and 2.37 eV, respectively.
Publisher
KOREAN FIBER SOC
Issue Date
2011-06
Language
English
Article Type
Article
Keywords

LIGHT-EMITTING-DIODES; TRANSITION-METAL CATALYSTS; METATHESIS POLYMERIZATION; ELECTRICAL-CONDUCTIVITY; CONJUGATED POLYMERS; POLYACETYLENE; EFFICIENCY; CYCLOPOLYMERIZATION

Citation

FIBERS AND POLYMERS, v.12, no.3, pp.291 - 295

ISSN
1229-9197
DOI
10.1007/s12221-011-0291-1
URI
http://hdl.handle.net/10203/98272
Appears in Collection
CH-Journal Papers(저널논문)
Files in This Item
There are no files associated with this item.
This item is cited by other documents in WoS
⊙ Detail Information in WoSⓡ Click to see webofscience_button
⊙ Cited 3 items in WoS Click to see citing articles in records_button

qr_code

  • mendeley

    citeulike


rss_1.0 rss_2.0 atom_1.0