4
Modified-creep experiment of an elastomer film on a rigid substrate using nanoindentation with a flat-ended cylindrical tip

Choi, Seung Tae; Jeong, Su Jeong; Earmme, Youn-Young, SCRIPTA MATERIALIA, v.58, no.3, pp.199 - 202, 2008-02

5
Superstrength through Nanotwinning

An, Qi; Goddard, William A., III; Xie, Kelvin Y.; Sim, Gi-dong; Hemker, Kevin J.; Munhollon, Tyler; Toksoy, M. Fatih; et al, NANO LETTERS, v.16, no.12, pp.7573 - 7579, 2016-12

6
Time-dependent adhesion of a polydimethylsiloxane (PDMS) elastomer film to a flat indenter tip characterized using a cohesive-zone law

Mai, Nghia Trong; Choi, Seung Tae; Chung, Koo-Hyun; Lee, Seung Ryoon; Shin, Dong Kil; Earmme, Youn-Young, PHILOSOPHICAL MAGAZINE LETTERS, v.94, no.4, pp.242 - 250, 2014-04