In the present work, Mn and Cr were added to a commercial A356 (Al-7.0Si-0.38Mg-0.12Ti-0.02Sr in wt.%)-0.20Fe cast alloy to control the crystallization of beta-Al5FeSi. The tensile properties are compared in terms of the way the microstructures changed before and after the addition of 0.20Mn and 0.13Mn-0.13Cr. The addition of 0.20Mn causes the acicular P-Al5FeSi to be replaced by granular or skeletal alpha-Al(Mn,Fe)Si in solidification, and the additions of 0.13Mn-0.13Cr acts as an effective replacing element of beta-Al5FeSi. Moreover, the addition of 0.20Mn functionally improves the strength, and the addition of 0.13Mn-0.13Cr improves the strain as well as the strength compared to a commercial A356 cast alloy. (c) 2005 Elsevier B.V. All rights reserved.
Publisher
Elsevier Science Bv
Issue Date
2006-07
Language
English
Article Type
Article
Keywords

HEAT-TREATMENT; MG ALLOYS; AL; BEHAVIOR

Citation

MATERIALS LETTERS, v.60, no.15, pp.1880 - 1883

ISSN
0167-577X
DOI
10.1016/j.matlet.2005.12.042
URI
http://hdl.handle.net/10203/2229
Appears in Collection
MS-Journal Papers(저널논문)
Files in This Item
This item is cited by other documents in WoS
⊙ Detail Information in WoSⓡ Click to see webofscience_button
⊙ Cited 60 items in WoS Click to see citing articles in records_button

qr_code

  • mendeley

    citeulike


rss_1.0 rss_2.0 atom_1.0