Showing results 1 to 4 of 4
Effects of Al-2lTi-23Cr coatings on oxidation and mechanical properties of TiAl alloy Lee J.K.; Wee D.M.; Lee J.K.; Wee, Dang-Moon; Lee H.N.; Lee H.K.; Oh M.H., SURFACE & COATINGS TECHNOLOGY, v.155, no.1, pp.59 - 66, 2002 |
Indirect Evaluation of the Long-Term Oxidation Properties of Al-21Ti-23Cr and Al-37Ti-12Cr Coating Materials for TIAl Alloy Lee, Jae Kyeong; Kim, SH; Wee, Dang-Moon; Kumar, KS; Oh, MH, METALS AND MATERIALS INTERNATIONAL, v.14, no.6, pp.713 - 720, 2008-12 |
Spallation resistance of oxide scales on Alloy 617 enhanced by boron addition Jeong, Hyeonuk; Kim, Se-Ho; Choi, Wonseok; Choi, Pyuck-Pa, CORROSION SCIENCE, v.140, pp.196 - 204, 2018-08 |
The role of grain boundaries in the initial oxidation behavior of austenitic stainless steel containing alloyed Cu at 700 degrees C for advanced thermal power plant applications Kim, Ju-Heon; Kim, Byung Kyu; Kim, Dong-Ik; Choi, Pyuck-Pa; Raabe, Dierk; Yi, Kyung-Woo, CORROSION SCIENCE, v.96, pp.52 - 66, 2015-07 |