The outstanding tensile strength of Ni-rich high entropy superalloy fabricated by powder metallurgical process Kang, Byungchul; Kong, Taeyeong; Ryu, Ho Jin; Hong, Soon Hyung, MATERIALS CHEMISTRY AND PHYSICS, v.235, 2019-09 |