The effect of post weld heat treatment on the creep-fatigue behavior of gas tungsten arc welded 308L stainless steel

Cited 28 time in webofscience Cited 0 time in scopus
  • Hit : 311
  • Download : 0
Gas tungsten arc (GTA) weld joints were made from 308L stainless steel. The microstructure and phase transformation of the as welded and post weld heat treated (PWHT) weldments before and after creep-fatigue test were examined using transmission electron microscopy (TEM). The results show that the primary cyclic softening is replaced by primary hardening after high temperature PWHT, which is due to the rearrangement of dislocation and the relief of residual stress. The primary delta-ferrite mainly transformed into sigma phase during the creep-fatigue test, and the remaining amount of delta-ferrite depends on the PWHT and creep-fatigue test conditions. Further more, high temperature PWHT shows a tendency to retard the delta-ferrite to or-phase transformation, which in turn promotes the creep-fatigue resistance of the weldment. (c) 2006 Elsevier B.V. All rights reserved.
Publisher
Elsevier Science Sa
Issue Date
2006-07
Language
English
Article Type
Article
Keywords

SIGMA-PHASE; METALS; MICROSTRUCTURE; 600-DEGREES-C; PRECIPITATION; GROWTH

Citation

MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, v.427, no.1-2, pp.35 - 41

ISSN
0921-5093
DOI
10.1016/j.msea.2006.03.105
URI
http://hdl.handle.net/10203/89615
Appears in Collection
Files in This Item
There are no files associated with this item.
This item is cited by other documents in WoS
⊙ Detail Information in WoSⓡ Click to see webofscience_button
⊙ Cited 28 items in WoS Click to see citing articles in records_button

qr_code

  • mendeley

    citeulike


rss_1.0 rss_2.0 atom_1.0