The effect of reoxidation time during the preparation of Ni-loaded CsLa2Ti2NbO10 on the photocatalytic hydrogen production in water decomposition reaction

Cited 10 time in webofscience Cited 0 time in scopus
  • Hit : 216
  • Download : 0
The photocatalytic decomposition of water for H-2 evolution over 1 wt.% Ni/CsLa2Ti2NbO10 was investigated according to the reoxidation time during the preparation. The dependence of photocatalytic activity on the reoxidation time was examined by XRD, UV-Vis, TEM and TPR. With the increase in the reoxidation time, the H-2 evolution increased gradually. The maximum H-2 evolution (212 mumol/h g-cat) was observed when the catalyst was reoxidized at 200 degreesC for 2 h. It is because of the small particle size of 10nm and homogenous Ni/NiO distribution. The drastic decrease of photocatalytic activity for samples reoxidized for 4 h was due to the partial formation of NiO bulk phase and the growth of nickel particles. (C) 2003 Elsevier B.V. All rights reserved.
Publisher
ELSEVIER SCIENCE BV
Issue Date
2003-08
Language
English
Article Type
Article
Keywords

EXHIBITING ION-EXCHANGE; LAYERED PEROVSKITES; NI(II) PHASE; = K; OXIDE; O-2; H-2; DEPOSITION; MECHANISM; CATALYST

Citation

APPLIED CATALYSIS A-GENERAL, v.249, no.2, pp.375 - 384

ISSN
0926-860X
URI
http://hdl.handle.net/10203/250646
Appears in Collection
CBE-Journal Papers(저널논문)
Files in This Item
There are no files associated with this item.
This item is cited by other documents in WoS
⊙ Detail Information in WoSⓡ Click to see webofscience_button
⊙ Cited 10 items in WoS Click to see citing articles in records_button

qr_code

  • mendeley

    citeulike


rss_1.0 rss_2.0 atom_1.0